Dave Earley
-
Posts
28 -
Joined
-
Last visited
Dave Earley's Achievements
Advanced Member (3/3)
25
Reputation
Single Status Update
See all updates by Dave Earley
-
I am currently building a fiber blanket kiln using a steel dog kennel, 2x2x3 ft. Hopefully I will be able to finish firing these pots.
-
I just unloaded the kiln, cone 9 down top and bottom. Pot closest to flue exit was under fired and it looks like heavy reduction all over. I fired up to red heat with propane and then used waste oil nozzles which were hard to adjust for a neutral flame and temperature rise. The suction nozzles needed only 1 or 2 psi. I used about 20 lbs of propane and about 6 gallons of used motor oil. the pots were single fired with mostly a simple ash glaze. I think the fire box is a little small for the oil burner since I immediately had a 12 to 18 inch flame coming out.
-