Hi, I'm looking at a set of Nitride-Bonded Silicon Carbide shelves for my kiln for the obvious benefits. I've got a two questions that are holding me up at the moment.
1. Is there any reason I can't do mixed shelving in a single firing. I've got a Skutt 1227, so replacing all the shelves is a bit more expensive than I'd like to do at the moment, and there's only a few shelves that really need it.
2. For the crash cooling aspect.. How is crash cooling different than running a cone fire program where the kiln simply stops? Will I need to run a program to manage cooling with these? I'll only ever be firing to cone 6. -
-
8 hours ago, Dick White said:
Do not replace the 50 amp breaker with the required 60 amp breaker unless the wire is 6 ga. or better.
@Dick White should this say “if” not unless? I can’t tell if because it’s 6ga. it should be replaced. Thanks.
-
It is #6 copper wire for all three wires, this I know I confirmed with the electrician.
- Dick White and Bill Kielb
- 2
-
14 minutes ago, Bill Kielb said:
You should have: A 2pole 60 amp breaker,
It’s a 2pole 50 amp breaker. I’ll have this replaced before I fire it up
-
19 minutes ago, neilestrick said:
Only 120V from the breaker?
The electrician I used to run the wire installed a 14-50R receptacle, which blame falls on both parties for not clarifying that I needed the 6-50R. No problem, I got the proper outlet and switched it out. Problem, I hooked up two ground and one hot. Anyhow, just got those switched around and the outlet is now pulling 240V. Fingers crossed for a hot kiln.
-
8 hours ago, neilestrick said:
Which error code did you get? Might have a relay that's sticking when it gets hot. Does your kiln have 5 louvers at the top of the control box or 6? If it's got 5, then it uses the clear relays, and you can see if they're getting really dark and worn out.
ERR1 is the code
The relays are still clear for the most part, the 1-2 relay has a slight discoloration on one side, but still mostly clear
5 hours ago, neilestrick said:What voltage are you running it on, and do you have the correct elements for that voltage?
It seems this is the problem. Only getting 120V. Elements are correct - 240V 1 P
Thank you @neilestrick!
-
Thanks @neilestrick, ran the paper test all pieces of paper started to singe.
Yes the holes are 1/4” vent holes. The previous owner had drilled 8 in the top and 6 in the bottom. -
Hello!
I'm having trouble with my kiln getting up to temp. Haven't gotten it to fire up to temp at all.
I've replaced the elements, which were at least a decade old probably 15yrs, and have measured Ohms, Top to Bottom: 13.7,14,16, 16,13.7,13.7
There were way to many holes in the lid and floor which I'v temporarily plugged with clay until I get this sorted. Currently 3 top holes and 2 bottom holesKiln lid seems to have a tight fit, only one spot that would just take a slip of paper.
I did just notice today that it's running on a 50amp breaker and not the 60amp as listed in the manual.
What would be the next things to check?
Edit to add: Down draft vent system -
-
I purchased a used kiln from a rural area school, they were downsizing to a smaller kiln requiring less power and to be able to fire more frequently. There are some nasty looking pits in the a couple shelves from melted, clay/glaze/something that make me wonder if I should even use them. They definitely didn't fire past cone 6, which is all I intend to go to, but can this leftover fused gunk further compromise the shelf? I haven't fired the kiln yet, but I'm getting close to the first bisque load. Should I get a replacement?
There are also a few shelves with large patches of run glaze. I've been working on chipping that off, how thorough do I need to be? If there is a pin head spot of glaze under the kiln wash, should I take that out?
These are the worst of them.
If you could do it all over again – kiln shelves recommendations for a beginner? (yes, this is another post on shelves)
in Equipment Use and Repair
Posted · Edited by Ja.Sc.
Thanks Hulk,
I was running through all these threads late into the night trying to ingest all the separate factors for each shelf type, and weighing that against cost and my personal use scenario. So there was a lot of tab hopping.
It seems that standard cooling, where the kiln is off, and vent continues to run is within the range of acceptable cooling rates? If anything it would still cool more slowly than using all silicon carbide shelves, right?
Crash cooling would be taking additional measures to increase the rate of cooling? If that's the case, I don't think I'd need to be concerned, I'm not in a rush.
I'm thinking the biggest potential for trouble would be having two shelves of different heat loads on the same level, potentially creating uneven cooling, also easily avoidable.