Town of Edgar train depot sign from 1900's
Mark C. commented on Biglou13's gallery image in Browse Member Galleries
-
I to add a bit of water to my wax to this it. You have to be more careful then as it runs even easier. Mark
-
As noted alumina will not melt and needs to be handled properly. Over the years I stopped adding it to wax ( as it settles out) instead I dip my cut sponge in wax and dip it into a small bowl of alumina powder. You have to be careful it does not run down the pot. I usually only use alumina on 1/2 of the lidded form the top or bottom then just straight wax on the sponge on the other 1/2.This process is fast and precise . Let these two pieces dry before putting the lid on.Then after glazing I sponge the edge once more with a wet sponge to remove any glaze drops. If the glaze gets any hydrate on it it will be rough and dry so you need to be carefull Now as to your wax it burns off not runs off so thats not the issue. No matter what kind you use I use mobil Ceramul A from Laguna-I think its sold in small amounts as I buy it in 5 gallons buckets-I use one up very 5 years or so. As far as it running did that happen when you applied it? As thats the only time it can run down. Mark
-
From the album: pots pots pots
-
From the album: pots pots pots
The best art fair truck out there -
From the album: pots pots pots
my old cat arch hardbrick kiln-back in the early 70's This baby used some GAS named it- the goose -
From the album: pots pots pots
slow news day -
From the album: pots pots pots
clay shed on road -
From the album: pots pots pots
throw/trim room -
From the album: pots pots pots
Green room -
From the album: pots pots pots
salt fence post dog -
From the album: pots pots pots
porcelain mug-cone 11- 12 ounces. -
From the album: pots pots pots
bamboo lifter-porc-cone 11 -
From the album: pots pots pots
covered jar -porcelain cone 11 -
From the album: pots pots pots
older raku pot -
From the album: pots pots pots
wood fire jug-stoneware -
From the album: pots pots pots
copper red teapot cone 10 redution -
From the album: pots pots pots
triggerfish wall piece-cone 11 -
From the album: pots pots pots
salt jug -
From the album: pots pots pots
2 quart pitcher cone 11 porcelain -
From the album: pots pots pots
salt jug -
From the album: pots pots pots
community salt load at my salt kin -
From the album: pots pots pots