  1. drying a large slip cast item - still in the plaster form- is it better to leave it upside down to drop out or will it dry faster right side up?

    1. Show previous comments  3 more
    2. terrim8

      terrim8

      It seems to dry/absorb so slow- its still in there! It was the right SG too so I'll keep it right side up . I may have complicated it all by having a paper-plaster mix behind the solid wall.

    3. JohnnyK

      JohnnyK

      Can you send some pix?

    4. terrim8

      terrim8

      with the next try-  decided to start again- back to the model to remove any imperfections so it will be totally smooth & then I'll insure its a smooth one-shot pour for the plaster.

       

×
×