  1. I wish there was an easy way to turn a caternary arch kiln into a salt kiln. I'm too lazy to rebuild it so I guess driving across the province to a salt kiln is my only option right now.

    1. Mark C.

      Mark C.

      Any catenary arch can be a salt kiln-conversions are easy.The main idea is to have some salt ports cut into kiln