  1. hitchmss

    7.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  2. hitchmss

    6.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  3. hitchmss

    5e.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  4. hitchmss

    5d.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  5. hitchmss

    4a.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  6. hitchmss

    4.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  7. hitchmss

    3.jpg

    From the album: All kinds of ceramic related stuff

    Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.
  8. From the album: All kinds of ceramic related stuff

    Thrown Stoneware, numerous dipped/sprayed glazes, gas fired, cone 10 reduction.
  9. From the album: All kinds of ceramic related stuff

    Thrown Stoneware, numerous dipped/sprayed glazes, gas fired, cone 10 reduction.
  10. From the album: All kinds of ceramic related stuff

    Thrown stoneware, thick slip decoration, numerous dipped/sprayed slips & glazes, gas fired, cone 10 reduction, soda.
  11. From the album: All kinds of ceramic related stuff

    Thrown stoneware, thick slip decoration, numerous dipped/sprayed slips & glazes, gas fired, cone 10 reduction, soda.
  12. From the album: All kinds of ceramic related stuff

    Thrown porcelain, thick slip decoration, numerous dipped/sprayed slips & glazes, gas fired, cone 10 reduction, soda.
  13. From the album: All kinds of ceramic related stuff

    Thrown stoneware, thick slip decoration, numerous dipped/sprayed slips & glazes, gas fired, cone 10 reduction, soda.
  14. From the album: All kinds of ceramic related stuff

    Thrown sections, glaze fired together. Early attempts to make larger work. Salt Fired. One piece got dropped, obviously.
  15. From the album: All kinds of ceramic related stuff

    Early attempts at larger work; thrown sections, which were glazed together.
  16. hitchmss

    10.JPG

    From the album: All kinds of ceramic related stuff

    A soda firing at Miami U.
  17. hitchmss

    9.JPG

    From the album: All kinds of ceramic related stuff

    A soda kiln before firing.
  18. hitchmss

    7.JPG

    From the album: All kinds of ceramic related stuff

    Teapot before perforation.
  19. hitchmss

    6.JPG

    From the album: All kinds of ceramic related stuff

    A soda kiln before firing.
  20. hitchmss

    5.JPG

    From the album: All kinds of ceramic related stuff

    Soda kiln after firing.
  21. hitchmss

    4.JPG

    From the album: All kinds of ceramic related stuff

    Soda kiln after firing.
  22. hitchmss

    3.JPG

    From the album: All kinds of ceramic related stuff

    Soda Kiln after firing.
  23. hitchmss

    1.JPG

    From the album: All kinds of ceramic related stuff

    Some real gems out of this kiln load.
  24. From the album: All kinds of ceramic related stuff

    Early work, thrown and assembled, thick slip decoration, sprayed glazes, gas fired cone 10 reduction.
  25. From the album: All kinds of ceramic related stuff

    Early work, thrown and assembled, thick slip decoration, sprayed glazes, gas fired cone 10 reduction.
×
×