Posts
839 -
Joined
-
Last visited
Content Type
Profiles
Forums
Gallery
Everything posted by hitchmss
-
From the album: All kinds of ceramic related stuff
Handle of the perforated tea pot; custom made die, extruded hollow handle. -
From the album: All kinds of ceramic related stuff
Extruded hollow spout, custom made die. -
From the album: All kinds of ceramic related stuff
One of my perforated tea pots; EXTREMELY fragile pots; You can see where I cracked it, but trying to move it around studio. -
From the album: All kinds of ceramic related stuff
Soda kiln in college; new stainless steel sides on the kiln. Still shiny! -
From the album: All kinds of ceramic related stuff
Soda kiln from college. In the midst of body redux. -
From the album: All kinds of ceramic related stuff
Soda kiln in college; spraying soda. Was also adding wood to fireboxes for fly ash. -
From the album: All kinds of ceramic related stuff
Spraying soda at kiln in college. -
From the album: All kinds of ceramic related stuff
Thrown bowl, thick slip decoration, numerous dipped and sprayed slips/glazes. Gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, thick slip decoration, numerous dipped and sprayed slips & glazes, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, thick slip decoration, numerous dipped and sprayed slips & glazes, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, thick slip decoration, numerous dipped and sprayed slips & glazes, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, thick slip decoration, numerous dipped and sprayed slips & glazes, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Some of my metalsmithing from college: "....Ring, ring, ring..." Fine silver. -
From the album: All kinds of ceramic related stuff
-
From the album: All kinds of ceramic related stuff
Another piece of my work from my college silversmithing; "...Forever, and ever..?" -
From the album: All kinds of ceramic related stuff
Another piece of my work from my college silversmithing; "...Forever, and ever..?" -
From the album: All kinds of ceramic related stuff
Another piece of my work from my college silversmithing; "...Forever, and ever..?" -
From the album: All kinds of ceramic related stuff
Thrown Stoneware, numerous dipped/sprayed glazes, gas fired, cone 10 reduction, Soda. -
From the album: All kinds of ceramic related stuff
Thrown Stoneware, numerous dipped/sprayed glazes, gas fired, cone 10 reduction, Soda. -
From the album: All kinds of ceramic related stuff
Thrown Porcelain, numerous dipped/sprayed glazes, gas fired, cone 10 reduction, Soda. -
From the album: All kinds of ceramic related stuff
Thrown Porcelain, numerous dipped/sprayed glazes, gas fired, cone 10 reduction, Soda. -
From the album: All kinds of ceramic related stuff
Thrown stoneware, gas fired, cone 10 reduction, soda -
From the album: All kinds of ceramic related stuff
Thrown stoneware, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda. -
From the album: All kinds of ceramic related stuff
Thrown porcelain, numerous dipped/sprayed slips & Glazes, gas fired, cone 10 reduction, soda.