From the album: Hope House International Fundraiser
Wheel-thrown, stoneware containers, approximately 12"-14" tall with the Hope House International logo stamped into the slab built handle on the lid. High-fired, Cone 10 with stain and Woo's Blue sprayed on exterior. Interior is glazed with Ohata Kaki.