Jump to content

ChenowethArts

Members
  • Posts

    687
  • Joined

  • Last visited

About ChenowethArts

  • Birthday 01/26/1950

Contact Methods

  • Website URL
    http://www.paulchenoweth.com
  • Skype
    paul_chenoweth

Profile Information

  • Location
    Kingston Springs, Tennessee - making pots out in the woods
  • Interests
    Ceramic Musical Instruments, Figure Sculpture, Handbuilt/Thrown-altered Pieces (with music themes). Paul sketches...probably has something to do with his architectural background.

Recent Profile Visitors

19,835 profile views

ChenowethArts's Achievements

Advanced Member

Advanced Member (3/3)

471

Reputation

Single Status Update

See all updates by ChenowethArts

  1. I opened up a bag of clay that I mixed, pugged, and wrapped over a year ago...I am more convinced than ever that age improves throwing (at least for the clay...hopefully for the maker).

    1. Show previous comments  1 more
    2. ChenowethArts

      ChenowethArts

      Roberta, I don't always let freshly mixed clay 'rest', but it seems to help the water content to become more homogeneous.

    3. Pres

      Pres

      Paul, I age all of my clay, but then freezing it in the Winter kills any bacteria/mold that may have started. Later though it is just fine. Aging does improve the clay.. immensely to me!

    4. Roberta12

      Roberta12

      Good to know. I had a couple of bags of clay in the garage that I had forgotten about during our 30 below season. They froze solid. While thawing out, they have gotten mushy. I just keep flipping the bags over and I will rewedge them at some point. Is that proper procedure?

       