  1. So I got busy and made three sinks for a house I am renovating. This past week I loaded them up and bisque fired them. One of the three survived the bisque firing. The good thing is I know how to efficiently make two more. Must allow more drying time for 1/2 inch thick ware this time..

    1. Show previous comments  4 more
    2. Denice

      Denice

      I need to make a couple of sinks someday. The ones in my bath are chipping. Denice

    3. Marcia Selsor

      Marcia Selsor

      My friend made sinks and made a bowl to fire them in an upright position.

    4. JLowes

      JLowes

      I have new clay for the remake of two sinks, it's a nice architectural clay , very groggy. This time I will take more time to dry, and punch some relief holes inside the foot ring near the foot/bowl join to let the water out better.

  2. JLowes

    Wynhill Pottery

    Work from Wynhill Pottery
  3. From the album: Wynhill Pottery

    Foil saggar fuming with copper wire wrap and wood chips
  4. I am getting loaded up for a show Saturday and Sunday in Norcross, Georgia. Just me, my honey, a hundred, or so, other artists and 50,000 people.

    1. Min

      Min

      How did your sale go?

  5. So I have half of my inventory I hope to take to my first show of Spring is in the kiln bisque firing. About two thirds are new designs I hope will sell well.

    1. JLowes

      JLowes

      So, only one unsatisfactory pot in the whole load. A handle detached itself at the top join. It looks like someone forgot to score and slip...oops. Need to decide how to go...handle...no handle. All the raku destined pieces from the load are fired and turned out well.

  6. Hello Florence W. THank you for your comment on my Avatar. It was inspired by my Yellow Labrador Retriever Lucy! She set me off on the raku animal quest, which is now my main direction for art/craft fairs and shows.

  7. From the album: Wynhill Pottery

    Raku fired clay with pink and grey underglazes beneath clear crackle glaze

    © @2012

  8. JLowes

    Ole Gator

    From the album: Wynhill Pottery

    Wall mountable alligator head figure

    © @2012

  9. JLowes

    Naked Raku

    From the album: Wynhill Pottery

    First Naked Raku pot fired in my homemade raku kiln. Resist clay layer made from same body as the pot.

    © @2012

  10. From the album: Wynhill Pottery

    Saggar fired pot with Horsehair & Ferric Chloride Fuming

    © @2012

  11. JLowes

    Autumn Fern

    From the album: Wynhill Pottery

    Saggar fired with ferric chloride fuming and fern frond from my backyard

    © @2012

  12. From the album: Wynhill Pottery

    Cone 6 stoneware mounted on a copper post

    © ©

  13. From the album: Wynhill Pottery

    Raku clay, raku fired, underglaze decoration unlder clear crackle glaze

    © ©

  14. JLowes

    Fat Cat

    From the album: Wynhill Pottery

    Raku clay, raku fired, underglaze decoration under clear crackle glaze

    © ©

  15. JLowes

    Yellow Dog

    From the album: Wynhill Pottery

    Raku clay, raku fired, underglazes under clear crackle glaze

    © ©

  16. From the album: Wynhill Pottery

    Earthenware with underglaze decoration under clear glaze. Designed for wall mounting.

    © ©