50ml Jug
9cm high. ES10 Stoneware Cone 9 (electric).
Quite pleased with the way the glazes turned out on this one, would appreciate your comments. Botz Tenmoku & Botz Satin Creme Matt
9cm high. ES10 Stoneware Cone 9 (electric).
Quite pleased with the way the glazes turned out on this one, would appreciate your comments. Botz Tenmoku & Botz Satin Creme Matt