Hulk

I had some buff clay to reclaim, and a small amount of speckled buff. I mixed them together. Uh-oh, major bloatware! The buff would take firing over cone 5, but minor problems start when fired over cone 5 and get worse with more heat work. The speckled buff seemed more tolerant going over cone 5. Together, eeh, no.

First few glaze fires in the new kiln, too much heat work, well over cone 6. This is more like it, left to right is top to bottom, where there's a five cone on each plaque, five & six where doubled up.

Credit

TM

Copyright

© TM

From the album:

Studio

· 8 images
  • 8 images
  • 0 comments
  • 5 image comments

Photo Information


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.