Grasses bud vase
Thrown porcelain. Wax resist all over, carved when leather hard. Black underglaze inlay painted over and wiped back. Bisqued to 1000oC. Orange underglaze highlights added. Transparent glaze poured and dipped then fired to cone 6/7.
Thrown porcelain. Wax resist all over, carved when leather hard. Black underglaze inlay painted over and wiped back. Bisqued to 1000oC. Orange underglaze highlights added. Transparent glaze poured and dipped then fired to cone 6/7.