Glaze Didn't Adhere


Recommended Posts

I put a coat of glaze on a pot last weekend. This weekend I went back to finish glazing. I dipped the same pot into another glaze. The second coat cracked and peeled off in chunks. It happened on 2 pots, same glazes. On one, i lightly tapped and brushed the loose glaze with a brush, then dabbed glaze back on with the brush.   - On the other, since is was more of a flat piece, I left it like that. I'm hoping it will still melt as I want it to even though it's cracked and not adhering to the first layer of glaze. 

I wonder if the first coat (dipped a week ago) got so dry the new glaze couldn't adhere. Other glazes adhered to the same first coat from last week though.

 So it might be just the two glazes don't work well together.

 

Does anyone have advice for me?

Thanks