paulw Posted June 5, 2014 Report Share Posted June 5, 2014 Hello, I am looking for a glaze that will give a "flat" black matte texture, not shiny. Any possible suggestions in a glaze or other unique ways to get this effect would be much appreciated. Thank you, Paul Link to comment Share on other sites More sharing options...
oldlady Posted June 5, 2014 Report Share Posted June 5, 2014 what temp? more details would help. Link to comment Share on other sites More sharing options...
Mark C. Posted June 5, 2014 Report Share Posted June 5, 2014 Cone 9 reduction?? Link to comment Share on other sites More sharing options...
Pugaboo Posted June 5, 2014 Report Share Posted June 5, 2014 Clay type and cone information is needed for anyone to be able to really help. Link to comment Share on other sites More sharing options...
paulw Posted June 6, 2014 Author Report Share Posted June 6, 2014 Hello, Thanks for the response. Will be firing at cone 10 and the clay soldate used for stoneware. All info appreciated. Paul Link to comment Share on other sites More sharing options...
bciskepottery Posted June 6, 2014 Report Share Posted June 6, 2014 Cushing Satin Black http://www.claybucket.com/2012/01/cushing-satin-matte-black.html Link to comment Share on other sites More sharing options...