Recommended Posts

Denice    243

Brian great video and a tightly stacked kiln, it probably took you hours. I think your firing turned out fantastic, every firing has it bleebs and cold and hot spot, well done. Denice

Share this post


Link to post
Share on other sites
Marge    0

Thanks for posting this great video. I actually learned alot by seeing how you packed your kiln and placement of witness cones. Thanks!!!

Share this post


Link to post
Share on other sites
Peter    0

Congrats on the new studio along with that exciting first firing. And thanks for taking the time to make this great video....

 

Peter

Share this post


Link to post
Share on other sites

I know you mentioned it - but I actually was VERY into your green! I am working on a pineapple jar and have had bad luck finding a good green color for it.

Share this post


Link to post
Share on other sites
Brian Reed    23

That glaze is super easy. I used a standard 4321 base and added .15% chrome oxide.

 

Custer Feldspar 40%

 

Silica 30%

 

Calcium Carb 20$

 

EPK 10%

 

Chrome Oxide .15%

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×