Hello,
Looking for information on the best way to make pendant lights shades. Thrown, slab or coils?

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,824 posts
  • LocationGrayslake, IL

Posted 14 February 2013 - 11:22 AM

All of those methods can work. Try to get them fairly thin- it makes it a lot easier to hang them. Make sure all the electrical connections are secure, with proper strain relief.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#3 GEP

GEP

    Moderator / full time potter ^6 stoneware

  • Moderators
  • 1,354 posts
  • LocationSilver Spring, MD

Posted 14 February 2013 - 01:33 PM

Have you considered using paper clay?

Mea
Mea Rhee
Good Elephant Pottery
http://www.goodelephant.com

#4 kathi

kathi

    Advanced Member

  • Members
  • PipPipPip
  • 51 posts
  • LocationCoastal North Carolina

Posted 14 February 2013 - 02:53 PM

I throw small cup-like vessels, trim the bottoms so that they are rounded and carve them. I get chain from Lowes and use that to support the weight (just like a regular hanging lamp). The chain comes in all sizes, so the appropriate weight is easy to find. Use small lamp kits (also available at the home improvement stores).

#5 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,216 posts
  • LocationWichita, Kansas

Posted 15 February 2013 - 09:37 AM

I have made many different pendants, wall sconces and lamps, keep them thin. The hanging light was thrown and then a design was carved out and that lighten it tremendously, wall sconces were slab and the lamps coiled. Using a shiny glaze on the inside will help reflect light into your room. Denice

#6 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 2,402 posts
  • LocationThe Hawkeye State

Posted 15 February 2013 - 05:47 PM

What about slip casting? Wouldn't that be an effective way, for making them quite thin?