Hey World,

 

I was reading this awesome article by steven hill about reduction look glazes at cone 6 in an electric kiln, but the firing schedule was for a kiln with a computer, and i have a manual kiln, how should i do this, i attached the recipie for the glaze and the firing schedule, thanks!

 

 

Darrel

post-13052-135856627568.jpg

post-13052-135856632195_thumb.jpg

post-13052-135856627568.jpg

post-13052-135856632195_thumb.jpg

Share this post


Link to post
Share on other sites
Mark C.    1,800

Its going to be a crap shoot at best but you WILL need a digital pyrometer and lots of time to babysit the kiln with a clock and a clear head. With your manual switch kiln try and recreate this schedule. every time will be an gamble on results.

I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.

Mark

Share this post


Link to post
Share on other sites
neilestrick    1,381

I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.

Mark

 

 

Bingo. Every show I go to has at least one potter making Steven Hill pots. While they are beautiful, they are just copies, and show very little creativity and certainly don't represent the personality of the potter. So if you do decide to use his glazes, figure out a way to make them uniquely yours.

Share this post


Link to post
Share on other sites
OffCenter    82

Before you go to all the trouble of doing a controlled cool down in a manual kiln, try just firing the Hill glazes one cone higher. I think you'll like the results.

 

Jim

Share this post


Link to post
Share on other sites
JBaymore    1,432

Instead of shutting the kiln completely off when the firing cone is down, turn all the elements to low for a couple of hours. See what you get. Likely you will be happy.

 

best,

 

.............john

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×