Jump to content


Photo

Steven Hill Glaze


  • Please log in to reply
5 replies to this topic

#1 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 18 January 2013 - 10:32 PM

Hey World,

I was reading this awesome article by steven hill about reduction look glazes at cone 6 in an electric kiln, but the firing schedule was for a kiln with a computer, and i have a manual kiln, how should i do this, i attached the recipie for the glaze and the firing schedule, thanks!


Darrel

Attached Files


Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#2 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 18 January 2013 - 11:05 PM

oops, here is the firing schedule.

Attached Files


Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#3 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,129 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 19 January 2013 - 01:34 AM

Its going to be a crap shoot at best but you WILL need a digital pyrometer and lots of time to babysit the kiln with a clock and a clear head. With your manual switch kiln try and recreate this schedule. every time will be an gamble on results.
I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.
Mark
Mark Cortright
www.liscomhillpottery.com

#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,906 posts
  • LocationGrayslake, IL

Posted 19 January 2013 - 09:46 AM

I suggest trying your own glazes and schedules with what you have. You may find the results could be great and they will be yours.
Mark


Bingo. Every show I go to has at least one potter making Steven Hill pots. While they are beautiful, they are just copies, and show very little creativity and certainly don't represent the personality of the potter. So if you do decide to use his glazes, figure out a way to make them uniquely yours.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#5 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 19 January 2013 - 09:58 AM

Before you go to all the trouble of doing a controlled cool down in a manual kiln, try just firing the Hill glazes one cone higher. I think you'll like the results.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#6 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,165 posts
  • LocationWilton, NH USA

Posted 19 January 2013 - 01:06 PM

Instead of shutting the kiln completely off when the firing cone is down, turn all the elements to low for a couple of hours. See what you get. Likely you will be happy.

best,

.............john

John Baymore
Adjunct Professor of Ceramics; New Hampshire Insitute of Art

Former Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com