I saw in a youtube video a guy using a plastic knife for shaping.
When I trim the top off of a pot I have difficulty using the long needle tool because of its lack of support, I use a thumb tack and get it right every time (the point is not too short because I tend to pull too thin rather than too thick)

What random objects have you used for tools and for what purpose?


Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, Montana State University-Billings

  • Members
  • PipPipPip
  • 4,298 posts
  • Locationwhere Texas, Matamoros, Rio Grande and Gulf of Mexico come together.

Posted 04 January 2013 - 12:52 PM

There was a long thread on a similar topic called " the proper inappropriate use of tools."

http://ceramicartsda...__fromsearch__1

Marcia

#3 Rebekah Krieger

Rebekah Krieger

    Advanced Member

  • Members
  • PipPipPip
  • 616 posts
  • LocationWisconsin

Posted 05 January 2013 - 01:09 AM

There was a long thread on a similar topic called " the proper inappropriate use of tools."

http://ceramicartsda...__fromsearch__1

Marcia



WOW- thanks for the link! It was a good read. I am especially interested in trying my cake decorating tools now after reading that thread!
Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#4 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 196 posts
  • LocationHarrisburg area, PA

Posted 07 January 2013 - 01:11 PM

I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!

#5 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 1,715 posts
  • LocationNorthern Virginia

Posted 07 January 2013 - 07:10 PM


I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!



http://finemessblog....-with-slip.html

http://finemessblog....i-tried-it.html

#6 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 1,892 posts
  • LocationThe Hawkeye State

Posted 07 January 2013 - 09:54 PM


I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....
"Anything worth believing, is worth questioning"

#7 Rebekah Krieger

Rebekah Krieger

    Advanced Member

  • Members
  • PipPipPip
  • 616 posts
  • LocationWisconsin

Posted 07 January 2013 - 10:33 PM



I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)
Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#8 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 1,715 posts
  • LocationNorthern Virginia

Posted 07 January 2013 - 10:38 PM




I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)





#9 Rebekah Krieger

Rebekah Krieger

    Advanced Member

  • Members
  • PipPipPip
  • 616 posts
  • LocationWisconsin

Posted 07 January 2013 - 10:59 PM





I am especially interested in trying my cake decorating tools now after reading that thread!


*grins* It's great fun once you get the right consistency of clay/slip. I also recommend perusing YouTube for gumpaste (fondant) flower tutorials -- sooo many techniques that should be adaptable to clay!


No need to adapt the techniques. Fondant is basically clay......at least it basically tastes like it....

LOL!! Try marshmallow fondant! It's not like the other plastic stuff! LOL
Also- I noticed that the clay dries pretty fast when trying to manipulate small pieces. Fondant retains it's moisture/ placidity. I have taken many cake flower classes and have som fondant stamps too! This could get fun! (now if only I could figure out how to make a lotus which was never taught in wilton courses! :-)



http://www.youtube.c...h?v=HrzoE7NzPOE


My mouth was literall agape the entire time! What the hell did I just witness!?! Holy cow! And by the way you win the award for finding literally everything I needed! LOL
Learning On my Kick wheel with my vintage Paragon (from the late 1960's)

#10 Nancy S.

Nancy S.

    My day job pays for my clay habit

  • Members
  • PipPipPip
  • 196 posts
  • LocationHarrisburg area, PA

Posted 08 January 2013 - 10:50 AM

http://finemessblog....-with-slip.html

http://finemessblog....i-tried-it.html


That's so freakin' cool!! So many ideas, so little time.... Posted Image