Posted 04 December 2012 - 09:19 PM

Hello


I want to be able to make spikes as large as possible by squeezing them with slip (I suppose dense could be nice).
I would like to do the slip from the clay (cone 04) I am using, I have darvan 811 and sodium Silicate (to reduce water content-shrinkage/crackings) but I don't know what quantity should I use, the formulas I find are for too big batches.

Is there some possibility to do about 2 pounds of slip?
THANKS!


#2 bciskepottery

bciskepottery

    Advanced Member

  • Moderators
  • 2,703 posts
  • LocationNorthern Virginia

Posted 04 December 2012 - 09:40 PM

Darvan will make the slip more fluid; you might want to use epson salt. Here's a good video that shows effects of using Darvan and epson salt.



#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,359 posts
  • LocationRed Lodge, Montana

Posted 04 December 2012 - 10:30 PM

Darvan will make the slip more fluid; you might want to use epson salt. Here's a good video that shows effects of using Darvan and epson salt.

http://www.youtube.c...player_embedded


great video!
Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 05 December 2012 - 12:38 PM

Deflocculating with Darvan or sodium silicate will allow you to take a VERY thick slip with low water content and make it fluid enough to work with, therefore minimizing shrinkage. Flocculating with epsom salts will take a slip with a higher water content and higher shrinkage rate and make it thicker, but will not do anything to reduce shrinkage.

I would take a very thick, sludgy, non-fluid slip, like almost thick enough to form into a shape, and deflocculate it by eye. Mix equal parts water and deflocculant and and add it a couple drops at a time to your sludge until you get the viscosity you need.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#5 Chantay

Chantay

    Advanced Member

  • Members
  • PipPipPip
  • 501 posts
  • LocationVirginia, USA

Posted 05 December 2012 - 12:44 PM

This is a great video. Should explain what you need to do. - chantay



- chantay

#6 claclana

claclana

    Advanced Member

  • Members
  • PipPipPip
  • 60 posts
  • LocationBuffalo, NY

Posted 05 December 2012 - 07:48 PM

GREAT!

I have the needed answer
Thanks!