So I just getting started with pit firing and I know that it isn't 'food safe' which is generally fine because I am more into making things like lanterns and wall masks. However I was wondering if a large bowl would still be safe for things like unpeeled apples and oranges or other fruits that have a peel on them. Also I have seen morter and pestle sets that seem to be unglazed. Are these safe to use for grinding herbs that will be used in food or not?

I'm sorry if these sort of questions have been answered, I didn't find them when I searched.

-winterlight

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,361 posts
  • LocationRed Lodge, Montana

Posted 27 November 2012 - 03:49 PM

It depends on a lot of things. First how thick or fragile is it? Did you bisque fire to 09 or 04? If it is thick it should hold apples without concern. It it has a delicate lip, and apple could chip it accidentally.
A wall mask should be fine.

Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 winterlight

winterlight

    Newbie

  • Members
  • Pip
  • 2 posts

Posted 27 November 2012 - 04:04 PM

It depends on a lot of things. First how thick or fragile is it? Did you bisque fire to 09 or 04? If it is thick it should hold apples without concern. It it has a delicate lip, and apple could chip it accidentally.
A wall mask should be fine.

Marcia



Thanks, I just mostly burnish and then I plan to fire it in a 3ft pit with sawdust and leaves on the bottom and stack wood on top. As far as rims go almost all of my work is very hardy. Delicate isn't really in my vocabulary, I like robust forms that don't look like they will break if I look at them wrong! I admire delicate work but it isn't in my repertoire!

#4 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,117 posts
  • LocationRaleigh, NC

Posted 27 November 2012 - 04:06 PM

I agree with Marcia but also ... I would not grind herbs or food in it since it will be soft and you will be grinding away the surface and eating it. Might be a little crunchy too. : - )
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#5 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 27 November 2012 - 04:55 PM

I would not use it for any food that could put moisture or oils into the pot, or anything that requires durability like a mortar and pestle.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#6 DAY

DAY

    Advanced Member

  • Members
  • PipPipPip
  • 160 posts

Posted 28 November 2012 - 08:40 AM

"Safe" has as many definitions as "Pretty".
Remember, for millennia people ate from wooden bowls, with wooden spoons. In Elizabethan times bathing was thought a highly risky endeavor.
As a decorative centerpiece, filled with fruit, a pit fired bowl is quite "safe'- but also quite fragile!

#7 Iforgot

Iforgot

    Advanced Member

  • Members
  • PipPipPip
  • 155 posts
  • LocationColorado

Posted 28 November 2012 - 09:11 AM

I'd say that in general pit fired work should be decorative, making a mortar and pestel would grid up your clay body. But you can make unglazed ware to be functional, if you fire with in 3 pyrometeric cone tempratures of your clay body's recomended vitrification point you will be fine.



Darrel
Derek VonDrehle

Raku, Pit fired, Majolica, and Stoneware ceramic artisit

#8 Denice

Denice

    Advanced Member

  • Members
  • PipPipPip
  • 1,271 posts
  • LocationWichita, Kansas

Posted 28 November 2012 - 10:24 AM

Try to use the lowest cone clay you can find or make when comes to pit firing. I have only been involved in a large Anazai pit firing and you could tell that every thing was so under fired that sneezing next to the pot could break it. I had a lot of work in the firing so I refired it to C 04 in my electric kiln, I lost some of the smoke patterns on the pieces but it was worth it to save the work. Denice

#9 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 5,051 posts
  • LocationGrayslake, IL

Posted 28 November 2012 - 12:39 PM

Remember, for millennia people ate from wooden bowls, with wooden spoons.


For millennia people also didn't know what bacteria was.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users