I just tried glass bead media for attempting to get a "mat" finish on a piece. It etched in further than I would like. Has anyone used walnut shell media?

Share this post


Link to post
Share on other sites
Mark C.    1,808

Depends on the glaze? How hard it is? (what its made of-like some colbalt glazes and reds are very soft)

what its fired to cone wise?

This may not be what you want to do but how about putting a Matt glaze on to begin with?

Walnut shells work great on painted wood and metal and are less aggressive than glass beads.

Mark

Share this post


Link to post
Share on other sites
Mark C.    1,808

I would try the shells and if its to aggressive enough add a very small amount of silica sand to them (small mesh size)

Mark

Share this post


Link to post
Share on other sites
buckbuck    3

Thank you. I will give it a try. I had to pick someting and got the glass bead. Next trip will be Walnut. Any suggestions if I have a choice on size? After I try it I'll post the results.

Share this post


Link to post
Share on other sites
Denice    243

You can find glass etching cream at craft stores all we have here is hobby lobby and Michaels. It's easier, cleaner and you can matt small areas with it. Denice

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×