Posted 23 April 2012 - 07:04 PM

He everyone. I'm using ^06 glaze on stoneware tiles I made, for my wooden table. No food will be eaten or prepared on the table top, so I just wanted to find out what without all think. Do I fire the glaze at ^06 or^ 6? Thanks in advance everyone. :)
P.s. I don't have access to the test kiln to test the results.

#2 atanzey

atanzey

    -

  • Members
  • PipPipPip
  • 147 posts
  • LocationSouth-Central Pennsylvania

Posted 23 April 2012 - 07:08 PM

If you fire cone 06 glaze to cone 6, it will melt off your tiles and fuse them to the kiln shelves. The maximum you can fire to is always the minimum temperature material.

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,144 posts
  • LocationRed Lodge, Montana

Posted 23 April 2012 - 08:27 PM

06 glazes at ^6 will run or blister and boil at the higher temperature. Go look at a Cone temperature chart. You are using a glazes that mature at 1830 or so to a temperature of 2230.
Marcia


Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#4 ThisIsMelissa

ThisIsMelissa

    Advanced Member

  • Members
  • PipPipPip
  • 30 posts

Posted 24 April 2012 - 10:46 PM

If glazes are 06, then that's as high as you can fire the glaze.
It will not vitrify the clay, however.

#5 esh

esh

    Newbie

  • Members
  • Pip
  • 6 posts

Posted 25 April 2012 - 01:23 AM

Firing to 06 obtains porous and relatively weak tiles, so it is recommended not to use the table for outdoor conditions.

#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,827 posts
  • LocationGrayslake, IL

Posted 25 April 2012 - 04:53 PM

Low fire glazes don't often fit well on stoneware clays. Potential for lots of crazing or even shivering. If you want to use low fire glazes, it's best to use a low fire clay.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]


#7 Surubee

Surubee

    Advanced Member

  • Members
  • PipPipPip
  • 38 posts
  • LocationNJ

Posted 26 April 2012 - 11:02 PM

Perhaps you could first fire the unglazed tiles to ^6 in order to vitrify the clay, then glaze them with your ^06 glazes and fire them the second time to ^06. This will mature the glazes without over firing them and the clay will be vitrified, too.

#8 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,827 posts
  • LocationGrayslake, IL

Posted 27 April 2012 - 09:18 AM

Perhaps you could first fire the unglazed tiles to ^6 in order to vitrify the clay, then glaze them with your ^06 glazes and fire them the second time to ^06. This will mature the glazes without over firing them and the clay will be vitrified, too.


You'll have a hard time getting the glaze to adhere to the vitrified tile during application. It's possible, but difficult.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

[email protected]





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users