clay lover    133

I have a Scott Creek Super Duper hand held extruder. I am longing for really small hollow extrusions, like less than 1 ".

 

Georgies has a hand held system with a hanger for suspending small center dies for tiny extrusions. Does anyone know if there is a way to adapt the Georgies center holder for the Scott Creek Gun?

 

Scott Creek doesn't make a hollow set up for their hand held gun and I have already invested in lots of dies for the Scott Creek gun and would love to be able to figure out a way to keep using it with the other center die suspender. Any ideas?

Share this post


Link to post
Share on other sites
Mark C.    1,807

Make a hollow extruder die for the small scott creek-not that hard to do-you can work in aluminum easy to bend drill or tap or file.

Mark

Share this post


Link to post
Share on other sites
clay lover    133

Mark, it's not the drilling, cutting ect that's stopping me, it's how to fasten the center piece to the rim piece. The center is about the size of a dime and too small to use u-bolts like I have used on hollows for the large wall extruder.

I talked to an aluminum welder and he wanted $100 to start the project! Stainless guy just as bad.

I can't think of another approach to holding the 2 pieces together. Any suggestions appreciated.

 

I'm wondering if the round die holder that Georgie's sell cold be made to fit the Scott Creek barrel, but they are only sold from Georgie's and I 've never had my hands on one to study it. The Georgie's rep just said, "I'm sure it won'd fit", but gave no reason why. Adaptation of that piece would solve the issue.

Share this post


Link to post
Share on other sites
bciskepottery    925

Take a look at how the bridge on the Northstar extruder dies work. You might be able for fashion something similar for yours, but on a smaller scale. You would not need a u-bolt.

Share this post


Link to post
Share on other sites
Mark C.    1,807

How about sanding the metal to roughen it up then clean it well and glue it with JB wield.That stuff should hold just about any stress.

Mark

Share this post


Link to post
Share on other sites
clay lover    133

JB Weld, not something I would have thought of. Worth a try. Thanks

I have some old cutting boards for making 1 piece dies for the big exptruder, I will think about the North Star approach to a smaller one.

Thanks, guys.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×