post-80534-0-67940400-1496950979_thumb.jpgpost-80534-0-88817800-1496951025_thumb.jpgits taken me over one year to get to my 1st pot  after being out of pottery for 11 years  the stone next to the porceal test is brownstone from wisconsin and is the same stone used to make the james J hill house . It was a popular stone from the 1800s i used it at 32% in the porcealinbody . along with 24 feldspar and 50% kaolin