Marcia Selsor Posted August 20, 2016 Report Share Posted August 20, 2016 This is a handout from my last #6 Reduction workshop in Corpus Christi. This is a word document Dan Engelke developed many ^6 reduction glazes at Lafayette University in the '70s and gave them out at an NCECA discussion group.I began working with ^6 reduction in 1980 when the ceramics lab was moved to a newer facility and the firings were supposed to fit into an 8 hours time slot. There is some repetition in this because of many pastings and adding. ^6recipes 2010 copy.pages.zip ^6recipes 2010 copy.pages.zip Link to comment Share on other sites More sharing options...
Guest JBaymore Posted August 20, 2016 Report Share Posted August 20, 2016 Thanks for sharing, Marcia. Link to comment Share on other sites More sharing options...
Denice Posted August 20, 2016 Report Share Posted August 20, 2016 Thanks Marcia for taking the time to post them. I'm sure your starting to pack for your big move. Denice Link to comment Share on other sites More sharing options...
Marcia Selsor Posted August 20, 2016 Author Report Share Posted August 20, 2016 Not yet. We're planning to move after the winter. But I am looking at "U-pack" options as we speak. It is suppose to be a long tough winter, but I do plan to start with moving the studio. Marcia Link to comment Share on other sites More sharing options...
Mark C. Posted August 21, 2016 Report Share Posted August 21, 2016 I cannot even grasp the thought of moving the studio. I wish you the best on that task. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted August 21, 2016 Author Report Share Posted August 21, 2016 I know. I went into my studio and took a photo. and walked out. Actually did some throwing but it is overwhelming. Debating on whether to keep my Soldner mixer. Marcia Link to comment Share on other sites More sharing options...
preeta Posted August 26, 2016 Report Share Posted August 26, 2016 marcia as a newbie who won't be continuing on to a 4 year college and who loves reduction this is far more precious than a diamond ring. mucho gracias. Link to comment Share on other sites More sharing options...
kev Posted August 27, 2016 Report Share Posted August 27, 2016 Thank you very much Marcia! I have only two years experience in this pottery making field so far but i really do love all aspects of it, especially the reduction glaze colors. I have several reduction glaze recipes so far that i like, i am very exited to try some of yours!! Link to comment Share on other sites More sharing options...