  1. I am in need of a few good books that have 1740-1790 ish pottery pictures for North America. Stoneware, red ware, earthenware. Mugs, tankards, plates and crocks are what my main interest is at this time. Any advice before I buy and just hope it’s a good book is much appreciated. Thanks.
  2. Leave the slop water in a 5 gallon bucket until it settles, pour off the cleanest water from the top and let whats left in the bucket evaporate. Sponges also help to suck up the clean water from the top. Reclaim the dry stuff thats left in the bottom of the bucket, i don't mix it with the good clay tho, it will have stuff from the floor in it.
×
×