What Can I Add To Make A Matt Glaze Glossy


Recommended Posts

Morning all,

 

I recently ordered a glaze which was available in matt and glossy.  I unfortunately did not specify the glossy code and the supplier did not check with me regarding the two options. I ordered 5kg and I really don't want to purchase another 5kg, as I had already made it up.  Can anyone suggest what I can add to this to make it glossy.

 

Thanks in advance

 

Andrea

Link to comment
Share on other sites

If you have a clear glossy, could test  over dipping a thin coat . I'd only do this on the top  third of a pot, or better on a test pot/tile.

Production glaze, have you the recipe?.

Even though this is disappointing maybe order hte glossy and play with the two similar glazes on pots, could be interesting:-00