AndreaB Posted May 6, 2016 Report Share Posted May 6, 2016 Morning all, I recently ordered a glaze which was available in matt and glossy. I unfortunately did not specify the glossy code and the supplier did not check with me regarding the two options. I ordered 5kg and I really don't want to purchase another 5kg, as I had already made it up. Can anyone suggest what I can add to this to make it glossy. Thanks in advance Andrea Link to comment Share on other sites More sharing options...
Babs Posted May 6, 2016 Report Share Posted May 6, 2016 If you have a clear glossy, could test over dipping a thin coat . I'd only do this on the top third of a pot, or better on a test pot/tile. Production glaze, have you the recipe?. Even though this is disappointing maybe order hte glossy and play with the two similar glazes on pots, could be interesting:-00 Link to comment Share on other sites More sharing options...
Marcia Selsor Posted May 6, 2016 Report Share Posted May 6, 2016 That is a good solution < Babs.I was trying to think of explains fluxes. Marcia Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.