docweathers Posted March 25, 2016 Report Share Posted March 25, 2016 I normally use silica 325 but I have some 200. Are there any situations in which 200 might be preferred to 325? Link to comment Share on other sites More sharing options...
MatthewV Posted March 25, 2016 Report Share Posted March 25, 2016 Yes, your wallet prefers the 200 mesh. If you are added silica to a clay body, the cheaper 200 will be fine. People have started using the 325 for glazes because it gives a slightly better finish. Link to comment Share on other sites More sharing options...
Mark C. Posted March 25, 2016 Report Share Posted March 25, 2016 It melts better than 200 so when you want a tad less met use the 200. I gave all my 200 to a glass artist years ago Link to comment Share on other sites More sharing options...