jrgpots Posted February 28, 2016 Report Share Posted February 28, 2016 The community challenge led me to explore tile techniques. If anyone here does encaustic tiles? If so please share your success and frustrations. Tips would be greatly appreciated. Jed Link to comment Share on other sites More sharing options...
oldlady Posted February 28, 2016 Report Share Posted February 28, 2016 contact angelica pozo in ohio. cleveland, i think. see her books on tile. she is a lovely lady and very helpful. Link to comment Share on other sites More sharing options...
bciskepottery Posted February 28, 2016 Report Share Posted February 28, 2016 http://www.potters.org/subject16159.htm Also check out Frank Giorgini and his book Handmade Tiles. Link to comment Share on other sites More sharing options...