dondon Posted October 17, 2015 Report Share Posted October 17, 2015 Hi, does anyone print their own decals from their own sketches for use on pottery? if so can you share the knowledge of how and what sort of printer and paper to use please? Link to comment Share on other sites More sharing options...
oldlady Posted October 17, 2015 Report Share Posted October 17, 2015 welcome to the forum. this was discussed recently, check for previous threads on the main page. i am not computer literate so cannot advise on how to find them i want to do the same thing so i will be interested in the answers you get. Link to comment Share on other sites More sharing options...
Judith B Posted October 17, 2015 Report Share Posted October 17, 2015 You have to use a laser printer but not all of them work, depends on the ink inside the cartridge and it works only for black as far as I know. I know the printer. The ones using cartridges hp85A (such as printer CE285AD) work. I don't know for the other ones. If you want colour decals, I suggest you send your designs to a printer. If you find the proper kind of printer, you should use CMC paper to print on. Link to comment Share on other sites More sharing options...
Valkyrie Posted October 17, 2015 Report Share Posted October 17, 2015 Justin Rothshank has some advice: http://rothshank.com/justins-work/decal-resources/ Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted October 17, 2015 Report Share Posted October 17, 2015 Send a pdf file to . http://www.foragestudios.com/decal-love/ Mariko Paterson makes them for others. Link to comment Share on other sites More sharing options...