Fusionous got a reaction from Chilly in How to prevent this from warping when glaze firing?
Thank you Min, Callie for your suggestion! I'm cautiously optimistic as the 2nd try worked! Here's the picture. Fired with pin setters beneath the 2 dips plus the sides!
-
Fusionous got a reaction from Callie Beller Diesel in How to prevent this from warping when glaze firing?
Thank you Min, Callie for your suggestion! I'm cautiously optimistic as the 2nd try worked! Here's the picture. Fired with pin setters beneath the 2 dips plus the sides!
-
Fusionous got a reaction from Kelly in AK in How to prevent this from warping when glaze firing?
Thank you Min, Callie for your suggestion! I'm cautiously optimistic as the 2nd try worked! Here's the picture. Fired with pin setters beneath the 2 dips plus the sides!
-
Fusionous got a reaction from Hulk in How to prevent this from warping when glaze firing?
Thank you Min, Callie for your suggestion! I'm cautiously optimistic as the 2nd try worked! Here's the picture. Fired with pin setters beneath the 2 dips plus the sides!
-
Fusionous got a reaction from Callie Beller Diesel in How to prevent this from warping when glaze firing?
Yes i will be trying out this method. Probably 2 points per valley to support. thank you!
-
Fusionous got a reaction from Callie Beller Diesel in How to prevent this from warping when glaze firing?
I have a cookie with holes which i can place pins in, so i will need to support the 2 valleys correct?