Venicemud Posted April 15, 2015 Report Share Posted April 15, 2015 I recently bought Lana Wilson's new DVD (as a reward to myself for finishing my income tax return) and noted that she uses paper clay to form pieces from her delightfully decorated slabs. It would be really fun to attempt some of Lana's techniques but I am restricted to the use of an electric kiln. Is the burn off of the paper in paper clay going to damage my kiln? Venicemud Link to comment Share on other sites More sharing options...
Mark C. Posted April 15, 2015 Report Share Posted April 15, 2015 No it will be fine. Mark Link to comment Share on other sites More sharing options...
Chris Campbell Posted April 15, 2015 Report Share Posted April 15, 2015 I agree with Mark ... It stinks while burning off but the kiln is fine. Link to comment Share on other sites More sharing options...
Venicemud Posted April 15, 2015 Author Report Share Posted April 15, 2015 Oh great, I'm so happy to read those reassurances from you two - people who I have thought of in the past as being amongst those who know what they are talking about. Lana Wilson's DVD by the way is a kick, she dissolves in laughter at the end and, although it was past my bedtime and I was tired, I found myself sitting there laughing out loud myself. Thanks. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.