Norm Stuart Posted January 29, 2014 Report Share Posted January 29, 2014 You're correct. Laguna Clay does not sell a product called Laguna Borate, even though that product may have existed at one time. I had assumed the Digitalfire article spoke of a current product - apparently not. I'm certain Tony Hansen knows this because he's paid to maintain Laguna Clay's Axner website. http://www.axner.com/gerstley-borate.aspx Laguna Clay owns the Gerstley Borate name and the huge remaining supply. The chemical composition of Laguna Clay Gerstley Borate in their PDF is very similar to the "Rationalized Gerstley Borate" Tony Hansen has on Digitalfire -- but is quite different to what Tony Hansen calls Laguna Borate and all other Gerstley Borate substitutes. I have no idea what "Rationalized Gerstley Borate" is, but it suggests Gerstley Borate from the original producer varied from bag to bag as the material was mined. I can only imagine the amusement Jon Brooks enjoys when reading twitterpated posts by envious competitors who can no longer sell Gerstley Borate unless they buy it from Laguna Clay. In many posts I've said I think Laguna Clay sells horrible quality red iron oxide, and you're better served buying synthetic red iron oxide from US Pigment. But give the devil his due, Laguna Clay is the only source of Gerstley Borate anywhere in the world and sells it at a very inexpensive price - we pay about $0.50 a pound and it works perfectly. Jon Brooks provides this PDF file to clarify the sort of misinformation often posted. http://www.axner.com/pdf/laguna/Chemical_Composition_of_Gerstley_Borate.pdf Gerstley Borate There have been rumors that this product would become unavailable very soon. Those reports are wholly inaccurate. The supply* will last for many years, and because it is a stockpile (not a changing source from an active mine) the chemical analysis will remain quite consistent. This product has also been tested in the traditional “Floating Blue†glaze (see image) and the results were excellent. *3,000 tons or 6,000,000 pounds as of 6/18/2011 As John Baymore often says, "Know your materials, people." That's Laguna Borate, Norm, not gerstley borate. !!! The Laguna borate is a sub like the gillespie borate is. By the way there are tons and tons of the actual Gerstley borate kicking around so it is important for people to migrate to the gillespie or the laguna borate as apparently you have wisely done. But you are going to confuse people when you keep calling the Laguna borate, gerstley borate. If you call a ceramic supplier and order Gerstley Borate you will get Gestley Borate. We have many ton's of it here. We also stock the Laguna borate and the Gillespie. Reports from most folks so the Gillespie is the better of the two subs but either is better than the original. Neil has a nice bit on why actual gerstley is not good http://neilestrickgallery.blogspot.com/2011/03/gerstley-borate.html Link to comment Share on other sites More sharing options...
timbo_heff Posted January 29, 2014 Report Share Posted January 29, 2014 Sorry to high-jack this thread, but this is important: Laguna Borate is their manufactured sub for gerstley borate : absolutely , 100% no doubt See the Laguna catalog !!!!!! : http://www.lagunaclay.com/catalog/pdf/lcc_dryraw.pdf Look at the list of materials there: it clearly says for Laguna borate: A specially formulated flux containing a high percentage of boron. This material mimics the fluxing characteristics of Gerstley Borate: " and even in the link you sent http://digitalfire.com/gerstleyborate/lagunaborate.html : if you read it it is quite clear that it is what I am saying: Laguna Borate Laguna Clay claims this is almost identical in every glaze they have tried and is less expensive than Gerstley Borate was.." "Laguna Borate has the distinction of being the least expensive substitute available. " Yes, the remaining stocks of of Gerstley are owned by Laguna: it is still sold by them and others as Gerstley Borate. The link you posted for the Gerstley B chem analysis is for of the remaining stuff that came from the mine: (in it they claim that is consistent, but we all know it's not very consistent) The stuff that is consistent is the manufactured versions ! Laguna started making the sub when everyone else did ... they then bought the remaining stocks of the natural stuff as well. On Tony Hansens page (http://digitalfire.com/gerstleyborate/substitutes.html) he shows the chem analysis of the manufactured subs, including Laguna Borate, vs the actual mined stuff. So Norm, if you have been ordering "Laguna Borate" from them, you are using the consistent manufactured sub, if you have been ordering "Gerstley borate" from Laguna then you are using the stuff from the mine. Both products say laguna on the bag: both are available, but are not the same material. Yes, it is a bit confusing,that's why it's important that people get the difference here, especially since so many people love the floating blue glazes! The long and short of it is : if you can buy the original mined GB, don't do it. Get one of the substitutes like Laguna B or Gillespie B: they do what you need and are the same bag to bag. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted January 29, 2014 Report Share Posted January 29, 2014 That underglaze recipe actually came from Val Cushing's handbook but is written as 25% Frit 3110, 25 epk and 25 stain. Total is 75. So it makes more sense to use 1/3, 1/3, 1/3. I have posted this here several times over the years as well as on Clayart. It works as a low fire underglaze but it will sometimes go higher depending on application and which stain is being used. Marcia Link to comment Share on other sites More sharing options...
Matt Oz Posted January 29, 2014 Report Share Posted January 29, 2014 Laguna did make a substitute called Luguna Borate but they discontinued it. Short PDF with announcement. http://www.lagunaclay.com/msds/pdf/3rawmat/adry/lagborate.pdf So that explains all the confusion. Link to comment Share on other sites More sharing options...
Norm Stuart Posted January 29, 2014 Report Share Posted January 29, 2014 Thanks for posting that, Matt Oz. So, there was a "Laguna Borate" product at one time, which is no longer sold. The Gerstley Borate I purchase from Laguna says Gerstley Borate on the bag - I can post a photo. The chemical make-up in the PDF file closely matches "Rationalized Gerstley Borate" on Digitalfire, but is quite different to Gillespie Borate and other substitute GB products. Laguna Clay made a smart move when they purchased the remaining supply after the manufacturer decided it was no longer worth their while to sell it. We like the original Gerstley Borate product and still buy it from Laguna Clay. Laguna did make a substitute called Luguna Borate but they discontinued it. Lame PDF with announcement. http://www.lagunaclay.com/msds/pdf/3rawmat/adry/lagborate.pdf So that explains all the confusion. Sorry to high-jack this thread, but this is important: Laguna Borate is their manufactured sub for gerstley borate : absolutely , 100% no doubt See the Laguna catalog !!!!!! : http://www.lagunaclay.com/catalog/pdf/lcc_dryraw.pdf Look at the list of materials there: it clearly says for Laguna borate: A specially formulated flux containing a high percentage of boron. This material mimics the fluxing characteristics of Gerstley Borate: " and even in the link you sent http://digitalfire.com/gerstleyborate/lagunaborate.html : if you read it it is quite clear that it is what I am saying: Laguna Borate Laguna Clay claims this is almost identical in every glaze they have tried and is less expensive than Gerstley Borate was.." "Laguna Borate has the distinction of being the least expensive substitute available. " Yes, the remaining stocks of of Gerstley are owned by Laguna: it is still sold by them and others as Gerstley Borate. The link you posted for the Gerstley B chem analysis is for of the remaining stuff that came from the mine: (in it they claim that is consistent, but we all know it's not very consistent) The stuff that is consistent is the manufactured versions ! Laguna started making the sub when everyone else did ... they then bought the remaining stocks of the natural stuff as well. On Tony Hansens page (http://digitalfire.com/gerstleyborate/substitutes.html) he shows the chem analysis of the manufactured subs, including Laguna Borate, vs the actual mined stuff. So Norm, if you have been ordering "Laguna Borate" from them, you are using the consistent manufactured sub, if you have been ordering "Gerstley borate" from Laguna then you are using the stuff from the mine. Both products say laguna on the bag: both are available, but are not the same material. Yes, it is a bit confusing,that's why it's important that people get the difference here, especially since so many people love the floating blue glazes! The long and short of it is : if you can buy the original mined GB, don't do it. Get one of the substitutes like Laguna B or Gillespie B: they do what you need and are the same bag to bag. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.