I have a Econo Model KR23.
220 V 3 full sections with jumper cables
I have just rewired the whole kiln and I am very new at this.
new switches, new jumper cables, new wire, and one new element(because one was broken).
 
I am doing the glow test and turning all switches on high, but for each section I only get the bottom element to glow (I have 6 elements in total and only 3 are glowing)
I know it's getting enough Volts from the plug, and there's continuity to the other sections.
is there anything I can check to get these elements working?
Thanks!
 
Link to comment
Share on other sites

Failing to find a circuit diagram ...

This page gives electrical specifications of (some?) K-models,  only the K230 models are listed as having  6 elements.
https://hotkilns.com/hk-pdfs/%3Asites%3Adefault%3Afiles%3Apdf%3Ak-old-instruct
 

Note:
Each section of the kiln has an input control switch provided on the instrument panel. The K Model kilns used a four way switch (Low-Medium-High-Off). The original switches that were used are no longer available; however, a replacement switch made by Arkless is available. When changing to this switch you must order the replacement kit. (A diagram comes with the switch telling you how to rewire).
[My emphasis, as I believe other switches are available which need to be wired differently.]

Link to comment
Share on other sites

Agree with @neilestrick, the switches are probably wired wrong. As noted by @PeterH, replacement switches have a different arrangement of the connections on the back of the switch. The functioning of the 4-way switches is: on Low, both elements are on, but connected in series for 1/4 the total power of the section. On Medium, only the bottom element turns on, for 1/2 the total power of the section. On High, both elements are on, but connected in parallel for full power. Though you have the switch turned to high, the wiring to the elements is as if it is on medium.

Link to comment
Share on other sites

1 hour ago, neilestrick said:

@Cersamic In looking at your photos it appears you have 2 elements per kiln section, and they are wired in series, correct?

That serial plate for just one section of the kiln, correct? And you have 3 sections?

Did you get the switches from L&L or somewhere else?

So looking at https://hotkilns.com/hk-pdfs/%3Asites%3Adefault%3Afiles%3Apdf%3Ak-old-instruct again  -- there are 2*KR23 (rings) and 1*K23.

Assuming 240V at full power (on one ring) R = V^2/W = 240^2/3500 = 16.46 ohms.

So at full power that's the two 32.7ohms elements in parallel. At 50% power that's 240v across one element. At 25% power that's 240v across the two elements in series.  

From https://hotkilns.com/sites/default/files/pdf/ARKLESS.PDF
image.png.b04aad88851de24cb5036f432dc07340.png

Link to comment
Share on other sites

All of these types of switches are different. Did the Robert Shaw switches come with a wiring diagram? If so post a picture of it. Otherwise, do you have a multimeter? With that you can figure out the correct wiring placement by seeing which terminals have continuity on each setting.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.