anniec9 Posted June 7, 2013 Report Share Posted June 7, 2013 I have bisqued some small items made using a Porcelain to the temp. advised on clay pack - Porcelain 1080c. and am now wondering if I HAVE to glaze them, or can I leave them bisqued? Link to comment Share on other sites More sharing options...
Pompots Posted June 7, 2013 Report Share Posted June 7, 2013 You don't HAVE to glaze them, if you like the look and it serves the purpose that you made them for. Some raw porcelain is very good looking, there are some artist that glaze only the inside of the piece and leave the outside raw, that is a great look. Link to comment Share on other sites More sharing options...
neilestrick Posted June 7, 2013 Report Share Posted June 7, 2013 I would fire them up to their max temp if you're going to leave them raw. It will be more durable and stain resistant. Link to comment Share on other sites More sharing options...