LadyLumpsClay Posted September 13 Report Share Posted September 13 Hi all, My pot was too large to dip in my clear glaze so I poured over. Where the pours overlapped it was thicker and I think this caused the crawling. Can I fix it with another glaze fire? Thanks! Quote Link to comment Share on other sites More sharing options...
Min Posted September 14 Report Share Posted September 14 Refires are always crap shoots but if you don't have anything to loose it's worth a try. I'ld suggest that if you have some thicker glaze (from the side of the bucket where the glazes dry out) take some of that and get it on the bare spots then refire in the coolest part of your kiln. Chilly and Rae Reich 2 Quote Link to comment Share on other sites More sharing options...