Ianna Posted February 6 Report Share Posted February 6 My slip-mixer has been lying dormant for a few years and I have recently been trying to resurrect the slip but it's so compacted at the bottom! I added Darvan and water but it's not budging. Does anyone have suggestions on how to extract the pancaked slip or revive it? It's Cone 5/6 Oriental Pearl slip from Laguna Quote Link to comment Share on other sites More sharing options...
Mark C. Posted February 7 Report Share Posted February 7 (edited) You could empty the mixer and let the bottom dry out and get it out that way and rehydrate it again in small pieces. welcome to tne forum Edited February 7 by Mark C. Roberta12 and Magnolia Mud Research 2 Quote Link to comment Share on other sites More sharing options...