Keydecker Posted August 19, 2023 Report Share Posted August 19, 2023 I'm looking for a medium blue pint of commercial glaze that can be fired to cone 6 and not run! I tried coyote oasis and it really traveled. Is there a stable one out there? Any advice? Quote Link to comment Share on other sites More sharing options...
rox54 Posted August 19, 2023 Report Share Posted August 19, 2023 I used Amaco Potter's Choice Indigo Float a few years back and found it very easy to use. It really works well with texture too. JohnnyK 1 Quote Link to comment Share on other sites More sharing options...
JohnnyK Posted August 20, 2023 Report Share Posted August 20, 2023 Most of the Amaco Potters Choice glazes fire well without running unless you layer them. Then you just have to experiment to see what happens. Amaco's website has a lot of info regarding all of their glazes. You might also look at their Celadon glazes for something that might work for you... Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.