Niraja Posted June 7, 2023 Report Share Posted June 7, 2023 Hi. I am fairly new to ceramics. I have recently come across soda ash wash. However, I don't have the full understanding. What I understood in bits and pieces is sors give a somewhat soda-firing look. am I right on this part? if not then what does it do? Also, what are the different ways to apply soda wash? Love Niraja Quote Link to comment Share on other sites More sharing options...
Babs Posted June 7, 2023 Report Share Posted June 7, 2023 I have used it on unglazed bottom third of yunomi to get a toasty look, brushed on at bisqued stage. Be careful not to touch the washed area as the finish will be affected by this. I have only brushed, so can't comment on any othrr methods. Quote Link to comment Share on other sites More sharing options...
Min Posted June 7, 2023 Report Share Posted June 7, 2023 Hi Niraja and welcome to the forum! Have a read through of this thread, @Magnolia Mud Research has a really good post on using soda ash as a wash. Rae Reich and Magnolia Mud Research 2 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.