Al_ Posted June 6, 2023 Report Share Posted June 6, 2023 Would like to create a mirror finish on a sphere.. any suggestions appreciated please Quote Link to comment Share on other sites More sharing options...
Hulk Posted June 6, 2023 Report Share Posted June 6, 2023 (edited) Hi AI, Welcome to the Forum! For still damp clay, burnishing could help. Will the sphere be glazed? added: cover with very fine clay slurry, then burnishTerra Sigilatta (digitalfire.com) Edited June 6, 2023 by Hulk terra sigilatta link Quote Link to comment Share on other sites More sharing options...
JohnnyK Posted June 6, 2023 Report Share Posted June 6, 2023 If you are glazing and firing to cone 6, try 3 layers of Amaco's Potter's Choice "Palladium"... Quote Link to comment Share on other sites More sharing options...
Al_ Posted June 7, 2023 Author Report Share Posted June 7, 2023 Thank you so very much! Will give this a go! Appreciate your help! Have a wonderful day! Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.