Hi,

I have a one of a kind cup with a small hole in the side wall.

It's a kooky artsy yunomi type thing so can't really remake it, I know I should smash it but I love it.

I want to try the trick of filling with gold which I think is called Kintsukuroi.

Does anyone know how to do this?

Can i crumple up gold leaf and pack it in there?

Hoping Baymore San or one of you other masters out there might know.

I could fill with epoxy I guess but I doesn't seem right somehow.

Again, I know I should let go and smash it but I really would like to save it if possible.

 

Thanks!

Tim

Share this post


Link to post
Share on other sites

Hi,

I have a one of a kind cup with a small hole in the side wall.

It's a kooky artsy yunomi type thing so can't really remake it, I know I should smash it but I love it.

I want to try the trick of filling with gold which I think is called Kintsukuroi.

Does anyone know how to do this?

Can i crumple up gold leaf and pack it in there?

Hoping Baymore San or one of you other masters out there might know.

I could fill with epoxy I guess but I doesn't seem right somehow.

Again, I know I should let go and smash it but I really would like to save it if possible.

 

Thanks!

Tim

 

 

If I'm not mistaken the technique is actually using a laquer resin sprinkled with gold, not actually filling the cracks with gold...

 

I cant vouch for the efficacy or authenticity of the information contained in these links, but a google search yielded these:

http://nanbanceramics.wordpress.com/2011/08/17/86/

http://www.thewomensroomblog.com/2012/01/05/kintsugi-and-mottainai-nice-new-words-for-make-do-and-mend/

Share this post


Link to post
Share on other sites
Guest JBaymore

Tim,

 

Here I am......... ;)src="http://ceramicartsdaily.org/community/public/style_emoticons/default/wink.gif"> .

 

 

The technique is to glue the cracked pieces together or fill in the break with a layer of what ius called urushi (Japanese lacquer, and then do one of two things.......

 

One way the gold is added is to mix 24 karat gold powder with the urushi before the patching is done. This means that the gold appearance is throughout the lacquer repair. This is the more durable method,.... but the more expensive.

 

The second method is to let the surface of the urushi projecting on the surface of the piece to get partiallly dry and "tacky"..... and then press gold leaf onto the surface to put a thin layer of gold there. Cheaper, but easier to wear off.

 

It is VERY, VERY, VERY important to stress here that actual urushi is the sap from a plant/tree that is sort of related to Poison Ivy/Sumac... and gives you a HORRIBLE rash. Lacquerware apprentices in Japan suffer for years until they develop an immunity.

 

SO that being said.... here is the English language page for a small kit that is all you need to do this:

 

http://www.mejiro-japan.com/product/kintsugi-diy-set

 

 

It is not as easy as it sounds. Things like the humidity of the air will ghreatly affect the drying of the lacquer. As always........ test, test, test.

 

best,

 

......................john

Share this post


Link to post
Share on other sites

Tim,

 

Here I am......... ;)src="http://ceramicartsdaily.org/community/public/style_emoticons/default/wink.gif"> .

 

 

The technique is to glue the cracked pieces together or fill in the break with a layer of what ius called urushi (Japanese lacquer, and then do one of two things.......

 

One way the gold is added is to mix 24 karat gold powder with the urushi before the patching is done. This means that the gold appearance is throughout the lacquer repair. This is the more durable method,.... but the more expensive.

 

The second method is to let the surface of the urushi projecting on the surface of the piece to get partiallly dry and "tacky"..... and then press gold leaf onto the surface to put a thin layer of gold there. Cheaper, but easier to wear off.

 

It is VERY, VERY, VERY important to stress here that actual urushi is the sap from a plant/tree that is sort of related to Poison Ivy/Sumac... and gives you a HORRIBLE rash. Lacquerware apprentices in Japan suffer for years until they develop an immunity.

 

SO that being said.... here is the English language page for a small kit that is all you need to do this:

 

http://www.mejiro-ja...intsugi-diy-set

 

 

It is not as easy as it sounds. Things like the humidity of the air will ghreatly affect the drying of the lacquer. As always........ test, test, test.

 

best,

 

......................john

 

 

Can this technique work to repair glass?

Share this post


Link to post
Share on other sites
Guest JBaymore

Tim,

 

Here I am......... ;)src="http://ceramicartsdaily.org/community/public/style_emoticons/default/wink.gif"> .

 

 

The technique is to glue the cracked pieces together or fill in the break with a layer of what ius called urushi (Japanese lacquer, and then do one of two things.......

 

One way the gold is added is to mix 24 karat gold powder with the urushi before the patching is done. This means that the gold appearance is throughout the lacquer repair. This is the more durable method,.... but the more expensive.

 

The second method is to let the surface of the urushi projecting on the surface of the piece to get partiallly dry and "tacky"..... and then press gold leaf onto the surface to put a thin layer of gold there. Cheaper, but easier to wear off.

 

It is VERY, VERY, VERY important to stress here that actual urushi is the sap from a plant/tree that is sort of related to Poison Ivy/Sumac... and gives you a HORRIBLE rash. Lacquerware apprentices in Japan suffer for years until they develop an immunity.

 

SO that being said.... here is the English language page for a small kit that is all you need to do this:

 

http://www.mejiro-ja...intsugi-diy-set

 

 

It is not as easy as it sounds. Things like the humidity of the air will ghreatly affect the drying of the lacquer. As always........ test, test, test.

 

best,

 

......................john

 

 

Can this technique work to repair glass?

 

 

 

Probably..... you'd have to test it though.

 

best,

 

.............john

Share this post


Link to post
Share on other sites

My link I am curious. Just getting into ceramic's. I have very old ceramic fired hand-painted china done by my grandmother almost 50 years ago.

My link It looks

like oils on china but she also had gold fired on the edges. It is real gold leaf mainly on edges of plates. But my favorite plate had something heavy on it

and cracked in half. My husband glued it back but it left an ugly glue line. I am wondering if I can do the kintsukuroi on the break. But I think it may be

too late as the glue may be permanent. And I would like to try china painting. I do not have a kiln nor at my age want to invest in one. But I think

there are new classes in china painting. Where I could use their kiln.

Share this post


Link to post
Share on other sites

Tim,

 

Here I am......... ;)src="http://ceramicartsdaily.org/community/public/style_emoticons/default/wink.gif"> .

 

 

The technique is to glue the cracked pieces together or fill in the break with a layer of what ius called urushi (Japanese lacquer, and then do one of two things.......

 

One way the gold is added is to mix 24 karat gold powder with the urushi before the patching is done. This means that the gold appearance is throughout the lacquer repair. This is the more durable method,.... but the more expensive.

 

The second method is to let the surface of the urushi projecting on the surface of the piece to get partiallly dry and "tacky"..... and then press gold leaf onto the surface to put a thin layer of gold there. Cheaper, but easier to wear off.

 

It is VERY, VERY, VERY important to stress here that actual urushi is the sap from a plant/tree that is sort of related to Poison Ivy/Sumac... and gives you a HORRIBLE rash. Lacquerware apprentices in Japan suffer for years until they develop an immunity.

 

SO that being said.... here is the English language page for a small kit that is all you need to do this:

 

http://www.mejiro-ja...intsugi-diy-set

 

 

It is not as easy as it sounds. Things like the humidity of the air will ghreatly affect the drying of the lacquer. As always........ test, test, test.

 

best,

 

......................john

 

 

Can this technique work to repair glass?

 

 

 

Probably..... you'd have to test it though.

 

best,

 

.............john

 

 

John I think you might know but I've done a lot of research on this ... and what you say is true the worst thing is that the reactions is

 

TIME DELAYED BY UP TO THREE DAYS

 

so you can think it's fine and there is no reaction then three days later it's hive city!

 

I still have some repairs I need to do but I'll have on long gloves and a vapor mask.

 

I'm not really allergic to poinsen IVY, but this stuff is concentrated.

Share this post


Link to post
Share on other sites

Could this method be imitated somehow by filling the cracks with some other metal element? I have a beautiful platter that was fine in the bisque fire but in the glaze fire a huge wide crack opened up down the middle.... I want to fill it with a metal of some sort... but I have no idea how to do that. Any suggestions how would be appreciated. :)

Share this post


Link to post
Share on other sites
Guest JBaymore

Tim,

 

PMC shrinks a LOT from raw to fired. Not sure HOW that person gets this to fill in the spaces.

 

best,

 

...............john

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.