High Bridge Pottery Posted March 8, 2023 Author Report Share Posted March 8, 2023 Made up a 1kg batch with 1% bentonite added to see what it's like to throw with. Very rusty on my throwing so left it quite soft to make it easier. I tried a bowl first but that ended up flopping down so I put that on a plaster batt to dry out some more. First cylinder on the right was with the same really soft clay and the left one is the rewedged bowl. Seemed to throw about as well as the cone10 clay I used to work with. Might try another 1kg batch without the added bentonite and see if I can notice much difference. Can't find my good wood tool for cutting in the base Quote Link to comment Share on other sites More sharing options...
High Bridge Pottery Posted March 4 Author Report Share Posted March 4 Trying some frits as glazes, fired to 1100c (2012f) Kelly in AK and Hulk 2 Quote Link to comment Share on other sites More sharing options...