hlipper Posted October 29, 2022 Report Share Posted October 29, 2022 Hi all - just checked on my bisque firing (^04) and discovered an Err d on my L&L easy fire. Here are the specs: model number: e23S-240 serial number: 012607-F-CKG voltage: 240 phase: 1 I suspect I need new thermocouples and relays as I just replaced the elements. Any other recommendations? Also, can my L&L friend on here send me links to exactly what products I need? I emailed L&L 10 days ago (and followed up) and never heard anything. Thank you! Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 29, 2022 Report Share Posted October 29, 2022 Might be relays, might be thermocouples. How many firings are on them? If you turn the kiln on full power, do all the elements glow? Thermocouples HERE, assuming you have the standard type K. Relays HERE. Quote Link to comment Share on other sites More sharing options...
hlipper Posted October 29, 2022 Author Report Share Posted October 29, 2022 11 minutes ago, neilestrick said: Might be relays, might be thermocouples. How many firings are on them? If you turn the kiln on full power, do all the elements glow? Thermocouples HERE, assuming you have the standard type K. Relays HERE. Thank you, Neil!! There are about 100 firings on the thermocouples and relays. My elements gave out a couple weeks ago and we replaced them. The kiln is too hot right now to look but I did a luster ^019 firing last week and everything looked good. No issues with the elements. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 29, 2022 Report Share Posted October 29, 2022 22 minutes ago, hlipper said: Thank you, Neil!! There are about 100 firings on the thermocouples and relays. My elements gave out a couple weeks ago and we replaced them. The kiln is too hot right now to look but I did a luster ^019 firing last week and everything looked good. No issues with the elements. Could definitely be the thermocouples. Relays usually last more than 100 firings, but it's possible you have one that's sticking at higher temps. Quote Link to comment Share on other sites More sharing options...
hlipper Posted October 29, 2022 Author Report Share Posted October 29, 2022 11 minutes ago, neilestrick said: Could definitely be the thermocouples. Relays usually last more than 100 firings, but it's possible you have one that's sticking at higher temps. Great, thank you. Just ordered replacement parts. Somehow my kiln is back to running the program and is at almost 1800F...should I just let it keep firing or turn it off? Thanks!!! Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 29, 2022 Report Share Posted October 29, 2022 10 minutes ago, hlipper said: Great, thank you. Just ordered replacement parts. Somehow my kiln is back to running the program and is at almost 1800F...should I just let it keep firing or turn it off? Thanks!!! Let it run and see what happens. hlipper 1 Quote Link to comment Share on other sites More sharing options...
hlipper Posted October 30, 2022 Author Report Share Posted October 30, 2022 23 hours ago, neilestrick said: Let it run and see what happens. The program finished and I just unloaded the kiln this morning - everything looks good (hallelujah!). Hopefully I'll get the new thermos in early this week. Thank you again so so much for your help! Min and neilestrick 2 Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.