Have a look at the colourants used in this glaze.  Base glaze looks underfired but if you used those colourants in a well fitting clear it might be somewhere to start. Ceramic stains are great but they can lack the depth that using straight oxides can give. If it's too blue then I'ld try it without the cobalt. I'ld also swap out the iron chromate for chrome oxide + iron oxide so it's safer for you to use. (using the ratio of 70 chrome oxide with 30 iron oxide) Or just skip the iron and use 0.28 chrome oxide in the linked recipe.

Edited by Min
math
Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.