Rick Wise Posted July 27, 2020 Report Share Posted July 27, 2020 I have always fired my electric kiln to cone 6 with 4 peepholes closed and the 5th (top one) open all thru the firing. I have now installed an Envirovent II (downdraft venting system). Should I now fire with all holes closed? Link to comment Share on other sites More sharing options...
neilestrick Posted July 27, 2020 Report Share Posted July 27, 2020 With a downdraft vent, keep all the peeps closed. Link to comment Share on other sites More sharing options...
Sorcery Posted July 30, 2020 Report Share Posted July 30, 2020 Just don't forget to drill your top holes. Sorce Link to comment Share on other sites More sharing options...