Sorcery Posted July 24, 2020 Report Share Posted July 24, 2020 On 7/8/2020 at 8:36 PM, postalpotter said: Thanks to all! Sorcery, thanks for breaking things so I don't have to! I really don't produce enough to not make that a painful exercise! Mark, thanks again for helping to soothe my fears and arming me to fight off the gremlins. Neil, always safety first. Some of the neighbors are pretty sure I may blow-up the block! I broke some more things and found some carbon coring. Broke some old stuff and found less, but still existant carbon coring. Going to focus on a few more holds at specific temps to oxidize that. And leave the peeps open for max oxygen. Blow the block up! Sorce Last firing of "Debbiezula" results..... I kept all the peeps open, full primary and secondary air, full chimney/damper open till about 1900F on the Pyro then reduced. Ooooooo- it feels good! Last firing left, above firing right and Right! Sorce Link to comment Share on other sites More sharing options...