Old Salt Posted October 5, 2019 Report Share Posted October 5, 2019 Has anyone had experience using a NVS-07 Pugmill? Link to comment Share on other sites More sharing options...
Min Posted October 7, 2019 Report Share Posted October 7, 2019 If you type "Shimpo AND Pugmill" into the search box at the upper right corner of the page there are quite a few posts that come up. Not that specific one but it looks like @Babs has a Shimpo NVA-07, you could try pm her and ask for her thoughts on it if she doesn't see this thread. (to pm hit the envelope at the top of the page and follow the prompts) Link to comment Share on other sites More sharing options...
Babs Posted October 8, 2019 Report Share Posted October 8, 2019 Min of the amazing memory, yes I do!. Bought second hand from an old potter many years ago. Great machine heavy duty. I find taking it apart a major job now as the "barrel" is heavy for me now, always was but.. and bolt heads getting worn out. I rarely do this ,rather I keep in damp state..towels down the hopper and deairing orifice. Exruding end I seal really well. Hoping the grid part outlives me:-)) Gutsy machine. Link to comment Share on other sites More sharing options...
Old Salt Posted October 11, 2019 Author Report Share Posted October 11, 2019 Thanks, I like the specs of the machine, large hopper and 3 1/2" nozzle. about a year ago there was a pretty negative post about the pug mill. glad to know others like it. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.